RS00533R00FE12產(chǎn)品概述
Ceramic, Steatite or Alumina Core, Depending on Physical Size
Copper-Nickel or Nickel-Chrome Alloy Element, Depending on Resistance Value
Stainless Steel End Caps
Tinned Copperweld® Terminals
Complete Welded Construction
High Temperature Silicone Coating
Excellent Stability in Operation
Maximum Working Voltage: (P × R)1⁄2
Temperature Coefficient: ppm/°C, ±90 for 0-1 Ω, ±50 for 1-9.9 Ω and ±20 for 10 Ω and Above
Tolerance: 1%